Tools and Techniques for Measuring Coating Quality- Part 2, Moisture Detection
This is Part 2 of a 2-part series describing the instrumentation used to inspect the quality of cleaning and painting. Part 1 described the instruments used for determining the quality of cleaning and paint. Part 2 addresses moisture detection. The moisture content of the concrete should be determined prior to painting. In the author’s experience,
Tools and Techniques for Measuring Coating Quality- Part 2, Moisture Detection Read More »