Installation Woes of a Lining in a Demineralized Water Storage Tank
This month’s case from the F-Files concerns the application of a high performance liner in a steel demineralized water storage tank, or a demin tank. Demineralized (purified) water can be particularly aggressive in service when even minute traces of soluble salt contamination are present on a coated substrate. Therefore is not uncommon to see soluble
Installation Woes of a Lining in a Demineralized Water Storage Tank Read More »