Jay Helsel

cast iron coatings

Coatings for Cast Iron/Ductile Iron

Introduction – Cast iron and ductile iron can be coated with a variety of coating systems for both beautification and protection.   The selection of specific coatings depends on the service environment and the requirements for aesthetics. Coatings for cast iron are discussed below for general atmospheric exposure of cast iron surfaces and for underground exposure

Coatings for Cast Iron/Ductile Iron Read More »

Preparation of Cast Iron/Ductile Iron for Painting

By Jay Helsel, PE, KTA-Tator, Inc.  Introduction – Cast iron and ductile iron are two different materials but are prepared and painted similarly.  Ductile iron consists of iron, carbon, silicon, manganese, magnesium, phosphorous and sulfur, whereas ductile iron consists primarily of carbon and silicon together with nodular graphite to provide ductility. Ductile iron is commonly

Preparation of Cast Iron/Ductile Iron for Painting Read More »

Use of Fire Resistive Coatings in Building Construction

Fire resistive coatings generally refers to a broad group of materials known as sprayed fire resistive materials (SFRM).  These coatings provide protection to structural steel in buildings and other structures by serving as an insulative layer in the event of a fire.  The coatings are rated by how long they provide such protection, typically from

Use of Fire Resistive Coatings in Building Construction Read More »

steel intumescent coatings

Intumescent Coatings: A Review of Current and New Technologies

A commercial building’s structural support steel may not have exterior exposure, or even be visible inside the building, but in some cases — such as The New York Times building in Manhattan — it is part of the exterior facade. Visible or not, building codes generally require that structural steel be protected by a fire-resistive material,

Intumescent Coatings: A Review of Current and New Technologies Read More »

pinpoint rusting

The Case of Improperly Cleaned Surfaces: Failures in Preparation or Specification?

What happens if coatings are applied to an improperly cleaned surface? The simple answer might be to expect premature coating failure, but what exactly is an “improperly cleaned” surface? Was a contaminant left on the surface? Was cleaning not otherwise sufficient to meet the specified standard? Or was the specified coating not appropriate for the

The Case of Improperly Cleaned Surfaces: Failures in Preparation or Specification? Read More »

coatings for hospital

Selecting Coatings for Hospitals by Service Area

Coatings used in hospitals and healthcare facilities must be kept clean, which typically requires frequent scrubbing and disinfecting. These coatings must therefore be resistant to abrasion and to the chemicals used in cleaning products. Meeting these requirements typically indicates the need for high performance coatings. But there are often other requirements for coatings used in

Selecting Coatings for Hospitals by Service Area Read More »

Fireproof Coatings

Diagnosing Failure in Fireproofing [Intumescent Coatings]

The project specification for a recent building addition at a pharmaceutical manufacturing facility required that much of the structural steel be fireproofed. Fireproofing in this instance meant the application of a fire-resistive or intumescent coating. Intumescent coating products are designed to passively protect substrate materials—typically steel—from reaching combustion temperatures. These coatings function by charring and

Diagnosing Failure in Fireproofing [Intumescent Coatings] Read More »