phased array sectorial s scan

Changes to the 2015 Edition of the AASHTO/AWS D1.5 Bridge Welding Code

Background/Introduction

The AASHTO/AWS D1.5M/D1.5 Bridge Welding Code: 2015 published by the American Welding Society (AWS) covers the welding requirements for The American Association of State and Highway Transportation Officials (AASHTO) welded highway bridges fabricated from carbon and low-alloy constructional steels.

bridge welding codeThis code covers welding fabrication requirements applicable to welded highway bridges. The code is applicable to both shop and field fabrication of steel bridges and bridge components, and is to be used in conjunction with the AASHTO Standard Specification for Highway Bridges or the AASHTO LRFD (Load and Resistance Factor Design) Bridge Design Specifications. It has also been adopted by the railroad industry. This code is not intended to be used for Pressure Vessels or pressure piping, nor structures composed of structural tubing. 

Typically, the Bridge Welding Code is updated and re-published every 5 years to keep up with revisions to the AASHTO LRFD Bridge Design Specification, which is also re-published on a five-year cycle. Keeping the Bridge Welding Code on a five-year cycle maintains consistency with AASHTO LRFD.

Over the course of the 5 years, the AWS Bridge Welding Code Committee formally meets twice a year, with ad hoc committees meeting more frequently, The D1.5 Committee discusses changes in industry practices, new technology, requests for clarifications from users of the Code, and how these effects or change the current edition of the D1.5.  Revisions are presented and sent out for comments.  Comments are reviewed, discussed, and voted on by the D1.5 committee. Revisions that are accepted by the D1.5 Committee are advanced to the AWS Main Committee and if accepted, they are sent to AASHTO for their review and approval.  At any stage, proposed revisions can, and usually are, sent back to the D1.5 Committee for further consideration.  Modified revisions are sent back through the process, and when finally approved by all parties they are published in the next edition. 

The D1.5 Committee (formally known as D1J) consists of AASHTO representatives, industry leaders from both public and private sectors including bridge engineers from DOT’s, fabricators, manufacturers, consultants, Federal Highway Administration, and more.  The actual voting membership of D1J consists of 18 people.  The Committee is balanced with six members from AASHTO, six from AWS and six from industry.  The Committee is supported by numerous Advisors and Applicants that all contribute with their knowledge and experience.

The AWS Bridge Welding Code is recognized by all 50 states and many other regulatory agencies.

This article intends to highlight some of the changes made for the most recent 2015 Edition.

Changes: 2015 Edition

There are specific methods used to easily identify the changes made from one edition to the next.  A table in the Forward provides a summary of the “most significant technical changes.” Throughout the publication, changes are noted by a vertical bar on the left side of tables and figures; text changes are underlined.

Note from Forward:  This publication is justified by the need to monitor, revise, and update code provisions based on the needs of AASHTO member states and industry. The following is a list of the most significant revisions in the 2015 edition:

Additional Major Technical Changes to the 2015 Edition

  • 3 All approved PQR’s are valid indefinitely unless application of the WPS results in consistently substandard welds.
  • Clause 5.10.1 was re-written to reflect the change in the Fillet Weld PQR Testing:

5.10.1 Exemption from Groove Weld Qualification for Fillet WPS.  Groove weld testing is not required to qualify WPS’s for single pass fillet welds*.

*Single Pass Fillet Welds are exempt from Groove Weld Qualification PQR Testing.

  • Significant Heat Input Qualification Changes
  • Clause 5 Heat Input qualification requirements have been revised.
  • Voltage limits have been broadened.
  • A new amperage limit table for production qualification method has been added.
  • Prequalification based on restrictions in lieu of variables qualified by test has been removed.
  • Phased Array Ultrasonic Testing (PAUT) was added new to AWS D1.5 – 2015 Code:
  • 7.8 Phased Array UT (as described in Part C of this clause) in accordance with Annex K may be substituted for conventional UT.
  • Advantages of Phased Array UT Testing
  • Welds are ultrasonically examined by sweeping through multiple sound beams angles from 45 to 70 degrees refraction, which significantly improves detection of weld defects.
  • Encoding the scan allows for informative imaging and a permanent electronic record.
  • The combination of encoding and swept angles results in repeatability and makes it unlikely that an operator will miss a discontinuity.
  • Under the new Annex K, Primary Reference Level sensitivity is still the 1/16-inch diameter side drilled hole used for conventional UT.

PAUT may be substituted for RT when approved by the Engineer.

bridge welding code

ut scope a scan single angle
Example – UT Scope “A Scan” Presentation – Single Angle
phased array sectorial s scan
Example – Phased Array Sectorial “S-Scan” – Image Showing Multiple Angles

Removed from the 2015 Edition

  • Consumable Requirements
  • 6.1 Heat or Lot Testing. All welding consumables shall be heat or lot tested by the manufacturer to determine conformance with the requirements of this Fracture Critical Plan (FCP).

This sub-section was removed due to testing by Electrode Manufacturers that produce quality filler metal product under a continuing quality assurance program, audited and approved by one or more of the agencies described in 12.6.1.1 have proven that their quality is consistent, and no additional testing of the filler metal is required.

Summary

This article has highlighted some of the changes made in the 2015 Edition of the AASHTO/AWS D1.5M/D1.5 Bridge Welding Code. The Committee members’ and supporting personnel’s efforts and thousands of hours of volunteered time have resulted in an up-to-date Code that is referenced by tens of thousands of representatives of the bridge fabrication industry.  But it does not end there.  The same Committee (with a few changes to membership and support) has already been working on the next edition of the Code, as there will always be a need to correct errors, clarify ambiguities, keep pace with technology, and continue to improve the product.

Acknowledgement: Some information in this article was provided by David McQuaid – D.L. McQuaid and Associates and was used with his permission.