Introduction – Aluminum and aluminum alloys exhibit good corrosion resistance by virtue of a layer of aluminum oxide that forms on the surface.  While aluminum is often not coated because of its good corrosion resistance properties, there are occasions when coatings are applied to provide added protection in given environments (e.g., when the pH is

Cleaning and Painting Aluminum Substrates Read More »