The Ethics of Coatings Failure Investigations
“The Case of… Three (Consultants),” a two-part F-Files column published in the November and December 2010 issues of JPCL,1 described observations and conclusions reached by three different consultants, each looking at the same bridge coating system. The article pointed out that clients sometimes retain consultants to perform very specific and limited examinations of the alleged failing coatings. […]
The Ethics of Coatings Failure Investigations Read More »