Selecting an Adhesive for Tensile (Pull-Off) Adhesion Testing
Introduction One of the more frequently asked questions when it comes to testing the tensile strength of industrial protective coatings is, “What glue should I use to attach the loading fixture?” This brief article lists the stand...