galvanizing

Inspection of the Galvanizing Cleaning and Coating Process

Introduction – Hot dip galvanizing is cleaned and painted for both beautification and protection.  This coated galvanizing system is commonly called a Duplex System. In order for coatings to adhere and provide the desired service life, the quality of surface preparation and coating application must be assured.  This can be accomplished by thoroughly inspecting each …

Inspection of the Galvanizing Cleaning and Coating Process Read More »

galvanizing

Preparation of Galvanizing for Painting

You can listen to this article by clicking “Listen” and following along. Or, you can read the traditional way below. ________ Introduction – Hot dip galvanizing is painted for aesthetics or to capitalize on the synergistic effects of conventional paints to provide a protective barrier over the galvanizing, improving the longevity of the system.  Unfortunately, …

Preparation of Galvanizing for Painting Read More »